Abstract

Abstract An ABS polymer comprising (A) a graft copolymer formed by graft polymerizing styrene and acrylonitrile monomers onto an initially ungrafted, low gel diene rubber and (B) a copolymer of said grafted monomers in which said graft copolymer is dispersed; said diene rubber comprising 3 to 25% by weight of such polymer with the polymerized acrylonitrile content thereof being 27 to 40% by weight.

Inventors

  • 👤 Vincent A. Aliberti
  • 👤 Robert L. Kruse
  • 👤 Eduardo M. Valcarce

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 15:18
CPC Classifications
C; C08; C08F; C08F279/00; C08F279/02; C08F279/04

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 80 words
An ABS polymer comprising: (A) a graft copolymer formed by graft polymerizing styrene and acrylonitrile monomers onto an intially ungrafted, low gel diene rubber; and (B) a copolymer of said grafted monomers in which said grafted copolymer is dispersed; said diene rubber comprising 3 to 25% by weight of said polymer; the polymerized acrylonitrile content of said polymer being 27 to 40% by weight; said A and B simultaneously formed by continuous mass polymerization from a substantially uniform reaction composition.
Claim 2
Dependent Claim 80 words
An ABS polymer comprising: (A) a graft copolymer formed by graft polymerizing styrene and acrylonitrile monomers onto an intially ungrafted, low gel diene rubber; and (B) a copolymer of said grafted monomers in which said grafted copolymer is dispersed; said diene rubber comprising 3 to 25% by weight of said polymer; the polymerized acrylonitrile content of said polymer being 27 to 40% by weight; said A and B simultaneously formed by continuous mass polymerization from a substantially uniform reaction composition.
Claim 3
Dependent Claim 22 words
The polymer of claim 1 wherein the particle size of said diene rubber in said polymer is from 0.1 to 10 microns.
Claim 4
Dependent Claim 22 words
The polymer of claim 1 wherein the particle size of said diene rubber is from about 0.8 microns to about 10 microns.
Claim 5
Dependent Claim 23 words
The polymer of claim 1,2 or 3 wherein said diene rubber comprises from about 14 to about 25% by weight of said polymer.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-06-30 1989-12-30 1990-07-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-06-30 1993-12-30 1994-07-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-06-30 1997-12-30 1998-07-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag